Specification | Test | Standard | Royal Thin Brick® |
---|---|---|---|
Efflorescence | ASTM C-67 | None | None |
Modulus of Rupture | ASTM C-67 | 250 lbs./sq.in. | >500 lbs./sq.in. |
Compressive Strength | ASTM C-67 | No Standard | 10,000 lbs./sq.in. |
Absorption | ASTM C-67 | Max. 5% | <3% |
Saturation Coefficient | ASTM C-1088 | <8% – Waived | <3% – N/A |
Freeze-Thaw | ASTM C-67 | Min. 50 Cycles | Passed 3,000 Cycles |
Freeze-Thaw Brick in Concrete | ASTM C-666 Procedure B (as modified per PCI specification published April, 2007) | 150 psi or Greater | Passed 300 Cycles, Meets the Standard |
Shear Bond Strength to Portland Cement | ASTM C-482 | Min. 50 psi | >150 psi |
Chemical Resistance | ATSM C-650 | Not affected | Not affected |
Ironrock’s Thin Brick “Royal Thin Brick” shall be of standard grade quality and shall exceed all of the requirements of ASTM (American Society for Testing and Materials) C-1088, the standard specifications for thin veneer brick units made from clay or shale. The ASTM C-1088 standard specifications also require the ASTM C-67 Standard Test Methods for Sampling and Testing Brick and Structural Clay Tile as shown above.